Topic

eVent and steam iron

  • This topic is empty.
Viewing 6 posts - 1 through 6 (of 6 total)
PostedFeb 18, 2010 at 9:40 am

My eVent jacket care instruction tag says for best performance I should "steam iron warm to rejuvenate water repellent finish." Does anyone understand what this is supposed to do? And, iron it on which side – I've always assumed the outside but I thought the point of such a technical fabric was that vapor sized water could go from inside to outside but not vice versa. Anybody out there know how this works and why ironing would rejuvenate the water repellency?

Hiker 816 BPL Member
PostedFeb 18, 2010 at 10:11 am

Although the physics are a little bit beyond me, the ironing is to reactivate the DWR on the outside of the jacket, not to do anything to the eVent layer. So you definitely want to iron on the outside, not inside. Also, be VERY careful about the heat setting on the iron. Check this review that discusses potential problems with using too much heat.

Richard Nisley BPL Member
PostedFeb 18, 2010 at 11:02 am

A DWR works by creating a low attraction (surface energy) between water drops and the fabric. This allows the water drop to roll off rather than flatten out and stick to the surface.

The fluorochemical DWR molecules on the outer surface of your eVENT jacket contain a vinyl or acrylic polymer that sticks to the fabric. Attached to this backbone are little perfluoro tails (side chains) that are normally repelled from fabric surface by polar forces and stick up into the air. The little tails are what creates the low surface attraction to the water molecules and keeps the DWR working. Sustained exposure to water or abrasion will cause the tails to flatten out and the DWR to stop working. Heat of at least 140F is needed for about 15 minutes to create enough molecular motion for all of the tails to fully stand back up again.

Yes Hal, you iron the outside. For others using Nikwax or a Silicone DWR, heat will provide no benefit. In order of durability the above DWR type is the most durable, silicone is next, and wax is last.

Roger Caffin BPL Member
PostedFeb 18, 2010 at 12:57 pm

What Chris and Richard said about how a fluorocarbon DWR works.

Why 'steam'? In fact it isn't needed at all, but by specifying steam the vendor is trying to prevent you from having an iron that is red hot! That's all. Have the iron around boiling, not hotter, and skip the steam.

Cheers

PostedFeb 18, 2010 at 2:31 pm

Richard, Wow and thanks. Now I have another question. How did you know that? (Only on this website!)

Viewing 6 posts - 1 through 6 (of 6 total)